Aluminium alloys are frequently supplied and specified in a heat-treated condition — designated by a temper suffix (T4, T5, T6, T7, and others) that describes the thermal processing history that has been applied to the material after casting, extrusion, or forging. For industrial buyers specifying aluminium components, understanding what each temper designation means — and what mechanical properties and dimensional stability it delivers — is essential to writing a correct specification and to evaluating whether a supplier's delivered material meets the intended requirement. For aluminium suppliers and foundries, understanding the temper system is equally important: the wrong heat treatment sequence, or a heat treatment applied to an alloy that does not respond to it, wastes energy, adds cost, and may produce a component that meets the temper designation label while failing the underlying property requirement.

Which Alloys Are Heat-Treatable?

Not all aluminium alloys respond to heat treatment — only those whose alloying elements have sufficient solid solubility variation with temperature to allow precipitation hardening. The heat-treatable alloy families in common industrial use are the 2xxx series (Al-Cu), 6xxx series (Al-Mg-Si), and 7xxx series (Al-Zn-Mg-Cu) wrought alloys, and the casting alloys that contain magnesium as a strengthening element — most importantly LM25 (Al-7Si-0.3Mg, equivalent to A356) and LM16 (Al-5Si-1.3Cu-0.5Mg). The non-heat-treatable alloys — including LM6 (Al-12Si, no Mg), LM2 (Al-10Si-2Cu, low Mg), 5xxx series wrought alloys (Al-Mg), and 3xxx series (Al-Mn) — can be work-hardened (wrought alloys) or used in the as-cast condition but do not develop additional strength through thermal ageing. Specifying a T6 temper on an LM6 casting, for example, is a specification error — the alloy cannot respond to the T6 process and the component will not achieve the properties that T6 implies.

T4, T5, T6, T7: What Each Means

T4 designates solution heat treated and naturally aged: the alloy is heated to its solution treatment temperature (for LM25: 530–545°C for 8–16 hours), quenched rapidly in water, and then allowed to age at room temperature for a minimum of four days. Natural ageing develops moderate strength (LM25-T4: UTS approximately 200–230 MPa) with good ductility and toughness — a useful condition for components that will be subsequently formed or cold worked, or where ductility is prioritised over maximum strength. T5 designates cooled from an elevated temperature shaping process (casting or extrusion) and then artificially aged, without a separate solution treatment step. T5 is used for extrusions and die castings where the elevated temperature of the forming process itself provides partial solution treatment — a cost-saving shortcut that delivers intermediate properties (6061-T5 extrusion: UTS approximately 240–260 MPa) without the energy cost of a full solution treatment cycle. T6 designates solution heat treated and then artificially aged: the full two-step process that delivers maximum strength for heat-treatable alloys. For LM25-T6: solution treatment at 530–545°C, water quench, and artificial ageing at 160–170°C for 8–10 hours produces UTS of 280–310 MPa with elongation of 8–12% — the highest combination of strength and ductility available from this alloy. T6 is the standard temper for structural automotive and aerospace aluminium castings. T7 designates solution heat treated and over-aged beyond the T6 peak — typically at a higher ageing temperature or for a longer time than T6. Over-ageing reduces peak strength (by approximately 10–15% vs. T6) but significantly improves stress corrosion cracking resistance, dimensional stability at elevated temperature, and resistance to property degradation in service at temperatures above 100°C. T7 is specified for components that will operate in elevated temperature environments (engine components, heat exchanger housings) where T6 properties would degrade in service, and for components in corrosive environments where stress corrosion cracking is a design risk.


Back to Blog
RFQ
📄 Get a Quote